Phosphorus-deoxidised arsenical copper for parts that run hot under load, such as boiler stay bolts, firebox parts and heat exchangers.
Four controlled steps to a uniform arsenical copper.
Pure copper cathode (99.9% Cu) and clean copper scrap are selected and pre-heated to remove moisture.
Medium-frequency induction furnaces under a charcoal cover limit oxygen pick-up.
Arsenic (0.15% to 0.50%) is added and the melt is deoxidised with phosphorus. Chemistry is checked before pouring.
Water-cooled moulds produce dense ingots and billets.
Chemical composition standards, thermal limits, and physical properties of Arsenical Copper Alloy.
| Alloy | UNS | Copper (%) | Arsenic (%) | Phosphorus (%) |
|---|---|---|---|---|
| Arsenical copper (DPA) | C14200 | 99.40 min (with As and P) | 0.15 to 0.50 | 0.015 to 0.040 |
| Property | Value |
|---|---|
| Electrical conductivity | About 45% IACS |
| Thermal conductivity at 20 °C | About 190 W/m·K |
| Density | 8.94 g/cm³ |
| Product | Weight | Size | Bundle | Packaging |
|---|---|---|---|---|
| Ingots and billets | 20 to 35 kg | 600 × 100 × 75 mm | 1000 kg | Steel strapped pallet |
Key global industrial applications for High-Performance Copper Arsenic Alloys.
Stay bolts, firebox plates and steam parts under constant heat and stress.
Shells and tubes for heat transfer duty.
Evaporators, reaction kettles and acid-handling lines that need thermal efficiency.